Water, H2O is the most abundant compound on Earth's surface.

Contents

[edit] Optical properties

Refractive index 1.333 (at 0.5876 µm, 20 °C)

[edit] Other properties

Temperature,
°C
Density,
g/cm3
Cp,
J/(g·K)
Vapour
pressure,
kPa
Viscosity,
μPa·s
Thermal
conductivity,
mW/(m·K)
Dielectric
constant
Surface
Tension,
mN/m
0 0.99984 4.2176 0.6113 1793 561.0 87.90 75.64
10 0.99970 4.1921 1.2281 1307 580.0 83.96 74.23
20 0.99821 4.1818 2.3388 1002 598.4 80.20 72.75
30 0.99565 4.1784 4.2455 797.7 615.4 76.60 71.20
40 0.99222 4.1785 7.3814 653.2 630.5 73.17 69.60
50 0.98803 4.1806 12.344 547.0 643.5 69.88 67.94
60 0.98320 4.1843 19.932 466.5 654.3 66.73 66.24
70 0.97778 4.1895 31.176 404.0 663.1 63.73 64.47
80 0.97182 4.1963 47.373 354.4 670.0 60.86 62.67
90 0.96535 4.2050 70.117 314.5 675.3 58.12 60.82
100 0.95840 4.2159 101.325 281.8 679.1 55.51 58.91

(from [1] with corrections)

[edit] Refractive index database entries

[edit] External links

[edit] References

  1. Handbook of Optical Materials, Marvin J. Weber. CRC Press 2003